Stainless steel stamping parts processing production often uneven appearance problems, by the author tells us the main reason and processing method: 1.
There is no hole punch: in the process of processing stampings, workpiece internal air punch squeeze, can't eduction, result in artifacts appear uneven phenomenon.
Processing method is: punch to increase air flow.
2.
Stainless steel stamping blank uneven: billet surface uneven, lead to the workpiece surface is not flat.
Better processing method: replace the material surface.
3.
Material springback: elasticity, which leads to the workpiece is not smooth.
Methods: increasing annealing or plastic process.
4.
Material thickness tolerance is big, small thickness of the material, mold clearance slants big, lead to uneven shape.
Methods: the right replacement materials.
5.
Intensive large clearance, clearance when ambassador mold production leads to uneven effect on workpiece walls.
Methods: adjust the die clearance.
The above article is derived from the metal stamping parts, automotive stamping parts processing custom 18 years (
)
Original, reproduced please indicate the source.
【
Relevant recommendation 】
Details: how much do you know the new energy automotive stamping parts?
Details: sharing details of stamping processing industry: precision metal stamping parts figure how to draw, please be aware that this several steps